Pulsed Direct liquid Injection ALD of TiO2 Films Using Titanium Tetraisopropoxide Precursor
2013
Abstract TiO 2 thin films are grown by pulsed direct liquid injection atomic layer deposition with rapid thermal heating using titanium tetraisopropoxide and water vapor as precursors. The ALD growth rate is constant in the saturation zone range 35-47 ms at the temperature deposition of 280 °C. The TiO 2 growth rate of 0.018 nm/cycle was achieved in a self-limited ALD mode. SEM and AFM analysis showed the as-deposited films have a smooth surface with a low roughness. XPS analysis exhibited the stoichiometry of TiO 2 in the homogenous depth composition.